AirframeNovember 8, 2026· 9 min read

Aircraft Composite Structures: Damage Classification and Repair for A&P Exams

Composites are the one structures subject where the answer depends on a ply schedule instead of a rivet callout. The test asks what the damage is, whether it is inside a limit, and which repair the manual authorizes.

SL

SkyLicense Team

FAA A&P exam preparation specialists: helping mechanics earn their Airframe & Powerplant certificate since 2025

Where Composites Sit on the Airframe Test

Composite structure is subject AM.II.B, Non-Metallic Structures, of the Airframe ACS. The test is 100 questions in two hours at 70 percent. The sources are FAA-H-8083-31B Chapter 7, Advanced Composite Materials, with AC 43.13-1B Chapter 3 and Chapter 5. Our ACS syllabus guide maps the subject areas.

The Ply Schedule Is the Structure

A laminate is fiber in a resin matrix: fibers take the load, the matrix holds them and sets the service temperature. Fibers carry load only along their length, so the ply schedule is the structure. The handbook assigns 0 degree plies to axial loads, plus and minus 45 degree plies to shear and 90 degree plies to side loads. FAA-H-8083-31B states the rule: each damaged ply is replaced with a ply of the same material and orientation, because stacking sequence decides how the part carries load.

Allowable, Repairable, Beyond Repair

Three questions decide every composite discrepancy.

  • Allowable damage. Inside the allowable damage limit in the SRM. No repair, but record it and inspect at the stated interval.
  • Repairable damage. Outside the allowable limit, inside the repairable limit, so a published SRM procedure with a specified ply schedule applies.
  • Beyond repairable limits. Replace the part, or have engineering design the repair under approved data.

FAA-H-8083-31B adds repair life: temporary is limited by time or cycles, interim restores strength but not durability and carries a different inspection interval, permanent restores both. AC 20-107B frames the certification damage categories from barely visible impact damage upward. Paperwork follows: under 14 CFR 1.1 a repair is major if, improperly done, it might appreciably affect structural strength, or cannot be done by elementary operations.

Finding the Damage

Visual inspection finds most damage and misses the subsurface: delamination, disbonds, core crush, trapped water. Tap testing is the field screen. AC 43.13-1B paragraph 5-105 describes tapping with a coin or a light hammer of no more than 2 ounces against a known good area, and sets the limits: shallow defects only, skins thinner than 0.080 inch, no far side bondline evaluation without access to both sides, and no record produced. The handbook limits it to three plies or less.

Ultrasonic inspection follows. Pulse echo and through transmission both find delamination, porosity and bonding voids. Radiography reads density through the thickness, which suits water and metallic core, not a delamination parallel to the beam. A moisture meter reads radio frequency power loss, the usual tool for a radome or a wet sandwich panel. The NDI and NDT guide covers those limits.

Moisture and Core Damage

Water enters through a damaged skin, fastener hole, core edge close out or eroded leading edge. Most repair systems cure above the boiling point of water, so trapped moisture turns to steam and blows the skin to core bond apart. FAA-H-8083-31B states that core drying typically precedes any repair, by autoclave or vacuum bag. A Skydrol saturated core is worse: removal is described as almost impossible, and the contaminated core and adhesive come out.

Scarf, Step, Bonded, Bolted

Scarf and step joints are the flush geometries, and both spread load gradually. AC 43.13-1B 3-3 sets the light load laminate rules: scarf the hole edges about 50 times the thickness of the face ply, overlap successive patches by at least one half inch, add one extra ply for original strength. The handbook gives the same idea as a taper ratio, such as 1:40, or an inch of overlap per existing ply.

The step joint removes plies in a stair pattern: extend the cleaned out area by the number of plies removed less 1 inch, each layer 1 inch beyond the layer below, each successive layer one half inch inside the opening. Bonded repairs carry load through the adhesive and suit thin skins and sandwich facings. Bolts or blind rivets through an overlap patch suit thick structure. Core damage is commonly potted with paste filler, which AC 43.13-1B sets at 1 inch or less.

Wet Layup, Prepreg and Cure

Wet layup wets dry fabric with resin: simple, room temperature, lower properties than a factory part, so it dominates fairings. Prepreg arrives with resin in the fiber at a controlled ratio, is stored at 0 degrees Fahrenheit or below, and cures at 250 or 350 degrees Fahrenheit. Frozen material carries a storage life, typically six months to a year, and a mechanical life, the time out of the freezer before the resin advances.

Cure needs heat, pressure and a path for air. AC 43.13-1B paragraph 3-4 gives the stack: peel ply, bleeder plies for excess resin, a nonporous separator, breather plies to the vacuum probe, then the bag, at a minimum of 22 inches of mercury, with thermocouples at the repair. Bagging film must survive the cure, from polyvinyl chloride below 180 degrees Fahrenheit to polyvinyl fluoride at 450.

Lightning Protection and Fuel Tank Bonding

Carbon fiber conducts, resin does not, so a composite skin carries a manufactured path: copper or aluminum mesh, aluminized fiberglass, or conductive coating. FAA-H-8083-31B notes that the fine aluminum mesh corrodes around bolt and screw holes, degrades the panel electrical bonding, and is replaced to restore it. AC 20-53C adds that carbon composites have lower conductivity and need different design features, that adhesive bonding can reduce conductivity, and that tank bonding jumpers are part of the scheme. Shield bonding, sealing materials and structural foil shield liners are not to be left degraded or removed.

What the Exam Actually Asks

Four patterns: name the defect, telling a disbond from a delamination; choose the inspection method; decide whether it is inside a limit; pick the repair and its document. A plausible repair with no SRM reference is usually wrong, so quote the limit, not the technique. The sheet metal repair guide covers the metallic half of the subject area, and the corrosion control guide explains why that corroded mesh matters.

Start your FAA A&P exam preparation with SkyLicense free →

📥 Get the free printable study checklist: a 30-day FAA A&P exam prep plan with daily tasks covering 14 CFR Parts 43 and 65, AC 43.13-1B, ADs, and full-length exam simulations.

Download Free 30-Day Checklist →

Share this article

Want to check where you stand? Take a free FAA A&P practice test — General, Airframe and Powerplant, timed exactly like the real exam, with an explanation citing the reference for every question.

free FAA A&P practice test

Ready to train for your FAA A&P exam?

Exam-style questions, timed simulations and the theory for your General, Airframe and Powerplant ratings — pick your plan and start today. The FREE plan costs nothing.

Get Started

Create a free account